304 stainless steel turning in fact not difficult to imagine, as long as knives, cutting liquid selected, feel difficult.
1, stainless steel for the tool (W2) wear big, especially new workers, feeling bad deal, I plant observed turner sharpening time between stopping the machine caused, directly affect the yield, the choice of the United States ( Watts and special) 0.8R six-sided blade, and now the price at 38 yuan each flank only 6 yuan more than the benefits to be increased by 20%, down at the end of the turner of technical requirements to ensure quality.
2, cooling water is quite important, because high heat to bring 304 machining, tool damage, resulting in the buildup, the impact finish, be sure to choose stainless steel, special cutting liquid, the effect is obvious.
3, hole machining, tapping, do not be afraid, (1), the election stage a brand of wire work, drill pay attention to counterfeit, or you will be called "heaven." (2) to certain selected Tapping Fluid stainless steel, very easy, do not expect the oil, paraffin oil, that you are "old fashioned", who played in the 1970s stuff.
4, the last resort of a special process requirements, cutting difficult, choose 303 stainless steel, we drilled 75 deep with 2.5, all 304 stainless steel scrap, 303 of phosphorus, sulfur content, is easy to cut material, all issue more OK! !